2026-10-20 · 6 min read
Two quite different customers buy from our straight TIG wire family: toolrooms repairing moulds and dies, and fabricators welding 9Cr-1Mo-V heat-resistant steel. This article is about the first group. The second is a separate subject and deserves its own treatment, because the base metal and the procedure have almost nothing in common with tool steel repair.
The filler has to match the base metal
A repair weld in a tool is not a structural weld. The tool has to go back into service and take the same loads, at the same hardness, as the material around the repair — and a weld that is softer or harder than its surroundings becomes the next failure. That is why tool steel repair filler is chosen to match the base steel rather than to be generally suitable for steel. The whole selection reduces to identifying the base steel correctly.
Mould steel: P20
P20 is the pre-hardened mould steel most plastic injection moulds are cut from, and it is what our P20 wire is for. The point of a P20 repair is to restore the mould surface without a hardness step at the weld that will show up as a witness line on the part. Weld preparation and preheat matter here as much as the filler does.
Hot-work tool steel: SKD61 and H13
SKD61 is the Japanese designation for a 5% chromium hot-work tool steel; AISI H13 is commonly quoted as the equivalent, and DIN 1.2344 alongside it. Our listing groups SKD61, SKD11 and H13 together because in practice they arrive as one requirement from the same customer. That grouping is a supply convenience, not a claim that the three are the same steel — confirm the actual grade against the mill certificate before you choose a filler.
Hot-work steels are used for dies that see hot metal: die casting, forging, extrusion. They fail by heat checking and washout rather than by mechanical cracking, which is why the repair has to restore hot hardness and not just fill a hole.
Cold-work tool steel: SKD11
SKD11 is a high-carbon, high-chromium cold-work tool steel, used for punches, dies and cutting tools where wear resistance is the requirement. We are deliberately not quoting an AISI equivalent for SKD11 here: published comparisons do not agree with each other, and a filler chosen against the wrong equivalent is worse than no advice at all. Check the mill certificate on the actual tool, or send us the grade, and we will match against what the steel is rather than what a table says it might be.
Where preheating decides the result
Tool steels are hard, and hard steels crack when they are welded cold. Preheating slows the cooling rate at the weld and is the difference between a repair that lasts and one that cracks beside the weld a day later. The preheat and post-weld tempering temperatures are grade-specific and belong to the steelmaker data for that specific grade — we will not print a single number that is meant to cover P20, SKD61 and SKD11 alike, because no such number exists.
What we will do is confirm the filler against the grade you name, and tell you what we do not know rather than guess. A short message with the base steel designation, the tool type and the repair size is enough to start.
What we supply
Straight cut-length TIG filler wire in three entries: P20 for P20 mould steel, the SKD61 / SKD11 / H13 listing for hot-work and cold-work tool steels, and ER90S-B9 to AWS A5.28 for 9Cr-1Mo-V heat-resistant steel. Cut lengths and diameters outside the standard range can be quoted — ask rather than assume.
This article is a selection guide only. Preheat, interpass and post-weld heat treatment must follow the steelmaker data for the actual grade and your own welding procedure. The standard and the manufacturer technical file govern.